REPAIR OF METAL LOSS BY COLD WELD (BELZONA)

93 views
Skip to first unread message

Mohamed Elsahhar

unread,
Feb 20, 2016, 9:51:33 PM2/20/16
to materials-welding
dear members ,

i asked if repair codes or standers of pressure equipment allow to
repair metal loss in pressurized equipment with cold weld (BELZONA) if
allow it please give me your reference depending to ASME /API codes or
STD ,thanks for your time

Best Regards
QC/QA eng.
m.elsahhar

Samun Bhatia

unread,
Feb 22, 2016, 11:48:44 PM2/22/16
to material...@googlegroups.com

As per my view cold weld compound can not be used as substitue to weld built up. It is just used as cismetic work to facilitate coating or lining.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADGm7%3DzidsuSrdh%3DXmzuLgnZZNpRwWvQQVgao5s6_drgadCTgg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohd Siraj

unread,
Feb 28, 2016, 5:47:51 AM2/28/16
to Materials & Welding
As per API570 &510,
Reapir depend on thickness measurement.

permenant repair shall be done by flushing plate welding/hollow cylinder.

Temporary leak can b arrested by leak clamp.

Ramesh Bapat

unread,
Feb 28, 2016, 9:18:27 AM2/28/16
to material...@googlegroups.com
API 570, API 510
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8a835f29-6b91-44ca-b687-c88c59358831%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages