Can I write single WPS with two PQR . as per ASME sec IX

83 views
Skip to first unread message

venkateswara reddy Desireddy

unread,
Apr 24, 2025, 8:34:03 AM4/24/25
to material...@googlegroups.com
Dear experts ,
Can I write single WPS with two PQR .PQR are different process. onePQR SMAW & one PQR SAW


Regards 
D.V.Reddy

Deerendra Karanth

unread,
Apr 24, 2025, 9:43:06 AM4/24/25
to material...@googlegroups.com
Sir,
Yes, you can write a single WPS supported by two different PQRs with different welding processes, provided the following conditions are met as per ASME Section IX:

Code Reference:

ASME Section IX, QW-200.4(b): Attached for your
reference 

BR, 
Deerendra 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKmVceU4rJSYo5xdwsb_EO_eUJ3Jk3k9OU9RkoKGiACnPQ%40mail.gmail.com.
Screenshot_20250424-182033~2.png

Hany Nabil

unread,
Apr 24, 2025, 9:43:08 AM4/24/25
to material...@googlegroups.com

Yes 


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.


--

james gerald

unread,
Apr 24, 2025, 9:48:39 AM4/24/25
to material...@googlegroups.com
Inline image

You can combine 2 PQR's to form a WPS provided all essential variable & supplementary essential variables or same. In your case for combinin 2 processes, base metal and weld metal thickness range shall suffice.

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



--