TPI approval on WPS

700 views
Skip to first unread message

Venkat Ramana

unread,
Mar 21, 2020, 12:04:33 AM3/21/20
to material...@googlegroups.com
Dear Experts,

My query is that, is there any mandatory by TPI approval (Seal and Sign) on every WPS ?? even though they have already sign into the supporting PQR'S....

KINDLY CLARIFY WITH RELEVANT CODES AND STANDARDS.


Thanks & Regards

Venkat

Charles Jacob

unread,
Mar 21, 2020, 12:37:14 AM3/21/20
to material...@googlegroups.com
Dear,

As per ASME Sec IX 2019, there is no requirement of third party.all the clauses regarding review by authorized inspector has been repealed. So if you are qualifying according to 2019 edition,  third party sign and seal is not required.

Regards, 

Charles V Jacob 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.

Prakash Gotimukul

unread,
Mar 21, 2020, 12:37:14 AM3/21/20
to materials-welding
PQR and WPS are different.
WPS is procedure for performing the welding on jos. PQR is like performance test to check if this welding is possible. 
Rgds
Prakash Gotimukul
Consultant ASME/ISO/PED/IBR


--

k7moorthi

unread,
Mar 21, 2020, 1:24:57 AM3/21/20
to Materials & Welding
Hi,

Verify your Technical - Purchase order / Query issued by your client.

by
Kesavamoorthi Rajendiran.

Kannayeram Gnanapandithan

unread,
Mar 21, 2020, 3:00:00 AM3/21/20
to materials-welding
Not necessarily. But as per 2019, competent welding personal should be available to review welding related documents within company. 

--

harenath jha

unread,
Mar 22, 2020, 3:08:58 AM3/22/20
to material...@googlegroups.com
Yes , because every wps is an unique indentity

--

Venkat Ramana

unread,
Mar 22, 2020, 3:08:58 AM3/22/20
to material...@googlegroups.com
The contracted prepared and qualified as per AWSD1. 1 edition 2015 and ASME Sec IX edition 2015. Is there any requirement to do the sign on WPS copies??

Please clarify.... 

Venkat

Vinay Thattey

unread,
Mar 22, 2020, 3:08:58 AM3/22/20
to material...@googlegroups.com
Kindly see your PO conditions or tender condition . Is there any specific requirement of purchaser . TPI approval on every WPS is not envisaged.

--

Kannayeram Gnanapandithan

unread,
Mar 23, 2020, 5:36:33 AM3/23/20
to materials-welding
No. TPI can witness PQR and can review WPS. TPI can't Certify PQR and can't Approve WPS. In ISO as examining body, they can certify WPQR not WPS. 

Ramesh

unread,
Mar 23, 2020, 11:07:27 PM3/23/20
to material...@googlegroups.com
Each organisation can certify WPS/PQR. refer ASME Sec-IX- QW 201,  TPI review/witness is NOT mandatory,

TPI review / witness is Not code requirements, this is to satisfy customers that they have qualified WPS/PQR  upfront with third party check than vendors own personal. 

Also note, code allows SWPS - Prequalified WPS, means u can understand that does not require TPI involvement ! 


Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



NARK

unread,
Mar 24, 2020, 12:33:31 AM3/24/20
to Materials & Welding
Dear,

The TPI is not mandatory for the welder qualifications and welding procedure qualifications as per the code,if the client specification or contract  is mentioned any requirement ,then it become a mandatory requirement...

Regards

Nidhin r k 

james gerald

unread,
Mar 24, 2020, 3:13:16 AM3/24/20
to material...@googlegroups.com
TPI not a ASME Code requirement.

But it depends on Client Specification and Client Acceptance. Generally it is a practice to Qualify Welders &  PQR's with reputed TPI so that it can be Accepted by all Clients.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit

james gerald

unread,
Mar 24, 2020, 4:26:24 AM3/24/20
to 'james gerald' via Materials & Welding
Just to add,

If it a Heavy fabrication shop fabricating heavy equipments with ASME stamp you can use your AI.

If it is a plant construction site, normally client requires PQR qualified at site

Thanks & Regards

J.Gerald Jayakumar


Kannayeram Gnanapandithan

unread,
Mar 24, 2020, 4:26:25 AM3/24/20
to materials-welding
If it is code stamped equipment, TPI witness or approved WPS can not be used. It is the responsibility of manufacture

Kannayeram Gnanapandithan

unread,
Mar 25, 2020, 12:11:07 AM3/25/20
to materials-welding
Site is extension of stampholder. Quality system will have overall control. 

Vinay Thattey

unread,
Mar 26, 2020, 4:26:18 AM3/26/20
to material...@googlegroups.com

Prakash Gotimukul

unread,
Mar 26, 2020, 8:07:39 AM3/26/20
to materials-welding
For projects in middle east it is almost mandatory that a TPI is used although it is not a code requirement. In other countries u may follow what is prevailing in those countries.

Thanks & Rgds.
Prakash Gotimukul
Authorised Inspection Supervisor
AIA LLC TX USA
MOB +97155 7114671
           +919730039755

HENNING John

unread,
Mar 26, 2020, 11:13:03 PM3/26/20
to material...@googlegroups.com

If you are working to ASME no third party witness is required.  Your Authorized Inspector (AI) will definitely have involvement but they are not required to witness WPS involvement.

 

If you are working to AWS no third party witness is required.

 

If you are working to ISO 15614, third party witness by a Notified Body (NOBO) is required.

 

If you are doing structural work for Canada.   CWB witness is required and a retained Canadian Chartered Engineer is typically also required for companies operating outside of Canada.

 

If you are interested – my experience – hope it helps.

 

John

DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________

George Dilintas

unread,
Mar 30, 2020, 1:15:22 AM3/30/20
to material...@googlegroups.com
When PED (2014/68/EU) is applicable yes (see Annex I - 3.1.2), the NoBo has to approve the WPS,.
When ASME is applicable No. In ASME the manufacturer certifies the PQR, the WPS not

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsPJvRAQu5%3DeNN0L8qFX_-SjVMCK-YAkoQ2AjshHsBmPdw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages