Hi all I have one problem, if anyone have a solution these plz. give. I want to weld a tobe of wall thk. 5 mm. I want to acheive a weld of 20 mm od pipe on its wall with a controlled distortion of 0.01 mm. Can anyone please tell m which welding process I adope to acheive this. Please tell.
Tansu Ozcelebi (KREA)
unread,
Apr 4, 2009, 2:48:02 AM4/4/09
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
0,01 mm is not possible in welding method.