Imapct toughness testing on weld joint of material SA 516 Gr70

145 views
Skip to first unread message

Shahil Saini

unread,
Nov 10, 2020, 7:00:42 AM11/10/20
to material...@googlegroups.com
Hello everyone, 
Can anyone help me in finding out problems arising during impact toughness testing of the weld joint of the pressure vessel.

Thank you,

Customer Care

unread,
Nov 10, 2020, 10:35:56 PM11/10/20
to material...@googlegroups.com

Dear  Shahil,

In order to help you identify the problem, please report the following:

1. For the Charpy impact test, was the UG-84 ASME VIII-1 instructions followed?

2. What were the values of the impact test in ft-lb?

3. What was the test temperature?

4. Is the WPS qualified with the supplemental  Charpy impact test?

5. Regarding the sample: is the surface flat and does it appear shiny?

6. What welding process was used to make this pressure vessel?

7. The base material was selectionated as SA-516 Gr.70N?

 

Regards,

Ramon Briceno

www.linkedin.com/in/ramonbriceno-metallurgicalengineer

 

Sent from Mail for Windows 10

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8XbVQ6LfbHMXd4ymttDJ2ouSfT8jAn9GG0x_Q6uevnng%40mail.gmail.com.

 

Shahil Saini

unread,
Nov 11, 2020, 5:18:55 AM11/11/20
to material...@googlegroups.com
If the value of the impact toughness test does not match with the standard value, then what will be the further process?

Bien.ND |WIC

unread,
Nov 11, 2020, 10:45:43 PM11/11/20
to Materials & Welding
I agreed with Customer Care
Addition, I found problem in the PQR with actual test specimens that the subsize and reduction temperature not complied with UCS-66. You also check it out at UG-84.

Shahil Saini

unread,
Nov 15, 2020, 1:50:32 AM11/15/20
to material...@googlegroups.com
From where I get UCS-66 and UG-84?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Sourav Bohrays

unread,
Nov 16, 2020, 9:38:51 AM11/16/20
to material...@googlegroups.com
what is your equipment,what is code of construction ,reffer GA drawing,datasheet ...first know basic than step by step ..so what is your code of construction

Jamie Reyes

unread,
Nov 16, 2020, 9:38:59 AM11/16/20
to material...@googlegroups.com
If your question is inquiring about were you can find UCS-66 and UG-84, seek out Boiler and Pressure Vessel Code, ASME Section VIII Division 1, Rules for construction of pressure vessels.
You can purchase the latest edition for the above mentioned at www.asme.org 
Cheers.....

--
Regards,
Jamie Reyes