suppose i am going to weld 16 mm thick plate with single v groove butt weld for a length of 1 meter,
then how much kg of weld or electrodes is required?
apart from general triangular rule, is there any thumb rule?

RAJENDRA PRASAD TRIPATHI

unread,
Jul 27, 2015, 9:14:38 AM7/27/15
to Materials & Welding, nee...@gmail.com
For large Steel structure fabrication , it will be 2.5-3% of steel weight. Only for rough calculation.

Thanks
Vinay Tripathi

Saravanan Sornam

unread,
Jul 27, 2015, 11:09:35 PM7/27/15
to material...@googlegroups.com
Hi Neem Lal ,

Please find attached the Sample Calculation for Welding Consumable , which is derived from TWI.

Regards,
Saravanan

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2229b530-a9ee-432e-9d1d-b52f5e5ea14f%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

SampleWeldQtyCalculations.xlsx

K M JIJILAL

unread,
Jul 28, 2015, 12:23:53 AM7/28/15
to material...@googlegroups.com
Dear N.Lal ,
You are not mentioned the  degree of included angle.

Any how, by considering the angle is 60 degree , t=16 mm ,root gap =2mm and using downhill direction.The approx. no. of standard electrodes per meter joint shall be

Root Pass          - 3.15 dia.  - 7 pcs/mtr.
Filler +nup runs - 3.15 dia.   - 15pcs/mtr.
                          - 2.5 dia.     - 20pcs/mtr.



JijiLal K.M.,Welding Engineer,
Al banna Engineering LLC.
BPCL Kochi refinery expansion project.


Jiji Lal K M

issac

unread,
Feb 6, 2018, 5:43:54 AM2/6/18
to Materials & Welding
Dear Sir,

How you find this?/
can u tell me the formula which you use 

Regards 

Issac 

Rajesh Kasvala

unread,
Feb 6, 2018, 7:44:54 AM2/6/18
to material...@googlegroups.com
Find out you weld design area 


You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

BERNARDINO RODRIGUEZ

unread,
Feb 8, 2018, 12:09:22 AM2/8/18
to Materials & Welding
Look at this welding calculators. They may help you.

Best regards

sankar rao

unread,
Feb 9, 2018, 9:53:26 PM2/9/18
to material...@googlegroups.com
Dear sir 
Thumb rule formula

(Electrode diameter*40)+or - 20

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Hasin Shaikh

unread,
Feb 10, 2018, 8:43:37 AM2/10/18
to material...@googlegroups.com
whats unit kg or nos of electrode ?
--
*With Regards
Shaikh.Hasin
Email: hasin....@gmail.com
Mobile: +91-9924562942*


Rishikesh Kumar

unread,
Feb 12, 2018, 7:45:28 AM2/12/18
to material...@googlegroups.com
As per  below requirement for the amount of electrode requriement ,  this depends upon mainly your groove design. based on your groove design , the weld metal deposition  is calculated which include reinforcement also,
further   you should also have information related to  electrode to actual weld depositions. and then you can calculated all these values. 

 You may refer my  application   to get all these values very easily subjected to  you have such information with you.
the name of  application is " Smart welding Solutions" in andriod/iphone / Windows. its free of cost.

Hope these information will strengthen your welding activities.

 
Reply all
Reply to author
Forward
0 new messages