Blind thickness for hydrotest

629 views
Skip to first unread message

Ajay Paul

unread,
Feb 29, 2024, 7:49:50 AM2/29/24
to Materials & Welding
Dear Experts ,
        i need some clarification 
i need 50mm thickness blind for hydrotest,but i dont have that thickness so can i use welded  30mm+20mm blinds for it?
Pls. suggest .

Vinodchandra Bhatt

unread,
Feb 29, 2024, 11:04:20 PM2/29/24
to material...@googlegroups.com
Usually (as per code practice too), defined blind to be used. Sometimes plate blinds allowed with inspector permission but thickness can’t be achieved using layers. 

Thanks & Regards,

Vinodchandra Bhatt

On 29-Feb-2024, at 6:19 PM, Ajay Paul <ajay...@gmail.com> wrote:

Dear Experts ,
        i need some clarification 
i need 50mm thickness blind for hydrotest,but i dont have that thickness so can i use welded  30mm+20mm blinds for it?
Pls. suggest .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9e91e1e-4210-44a7-a40a-0cf05d968854n%40googlegroups.com.

Chiranjeevi A

unread,
Mar 1, 2024, 5:03:19 AM3/1/24
to material...@googlegroups.com, ajay...@gmail.com

thickness calculation for temporary blanks as per code B31.3  for your reference.

 

image.png

--

Mohan

unread,
Mar 2, 2024, 10:48:18 AM3/2/24
to material...@googlegroups.com, ajay...@gmail.com
Dear Team,

Please find the attached Plate made Blind Chart for easy reference.

Regards
G Mohanraj

Attachment A36 Temporay Blind Flange Thickness ASME Section VIII Divisio... (1).pdf