CS Normal pipe will be meeting the Specification(ASTM/ASME) standard
requirements.
NACE Pipes will be having additional restriction in Chemical
Composition,Hardness,Carbon Equivalent and Heat treatment
requirements.This additional requirements to ensure the usability of
material in Sour services
Regards,
pavainathan