Dear Sir,
Kindly clarify if  there is level III in PAUT&TOFD or not. our client insists for level III in PAUT&TOFD for PAUT procedure review and level II in PAUT&TOFD to carry out the work. i searched many but i found NO body has this certificates. are these certificates true? and how can i get it?

pgoswami

unread,
Feb 16, 2016, 11:09:17 PM2/16/16
to material...@googlegroups.com

Hi Mostafa,

 

These techniques are very specialized techniques. Not all NDE techs are up to speed with both of these techniques. Please see some guidelines from the BINDT on the same.

 

I’m not sure , where you’re located, you may check with the local high profile NDE Schools or Companies, who’ll have those personnel in their team

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/855091088.3944591.1455629104764.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Level_III_Brochure.pdf
PCN-GEN APPENDIX E9 ISSUE 7 REV A DATED 1ST JANUARY 2016.pdf

Santosh Gaikwad

unread,
Feb 16, 2016, 11:35:17 PM2/16/16
to material...@googlegroups.com
Dear Mr Mostafa,
There are so many Level 3 (PAUT & TOFD) are available in Market, for this technique certification body is BINDT .
As per ASNT there is no such certification available.  

you may  hire one level 3 as outside agency he will approve your procedure,

please find the attached document, in this document you can find your nearest training provider.

if any,  please feel free contact me   

Thanks & Regards.

Santosh Gaikwad

Surat,India.

ndt_ato.pdf

Shashank Vagal

unread,
Feb 17, 2016, 4:51:24 AM2/17/16
to material...@googlegroups.com
Hi,
PAUT, TOFD, etc are the techniques of UT method. If you have a Level III in UT, you may go for additional training for these techniques and be a so-called specialist. But mere training and certification may not make you competent, so to say to do justice to the job. You will master these techniques only by on the job experience by lot of practice on different types of test specimens.  
As such there is no specific Level III in this technique, but a UT Level III is qualified to write / review these procedures and a well experienced Level II individual can do the actual job. If required, the client may test him on a mock up test piece. This is the industry practice.
 
BR,
Shashank C Vagal 



From: pgoswami <pgos...@quickclic.net>
To: material...@googlegroups.com
Sent: Wednesday, 17 February 2016 5:08 AM
Subject: [MW:24310] RE: 24309] PAUT & TOFD Level III

Joseph

unread,
Feb 19, 2016, 1:47:17 AM2/19/16
to material...@googlegroups.com
Hi,

Level 3 certification in PAUT, TOFD, etc is issued by PCN BiNDT. There are Level 3's in these techniques.

Sent from my iPad

Prasad Ghanekar

unread,
Feb 19, 2016, 11:42:34 PM2/19/16
to material...@googlegroups.com

As I understand PAUT & TOFD are NDE UT technics and not NDE methods. Hence NDE Level III in UT is required with training in special technics.

Regards
P. V. Ghanekar

Shashank Vagal

unread,
Feb 20, 2016, 9:51:49 PM2/20/16
to material...@googlegroups.com
Again, let me stress this point: to master these techniques you need lot of on the job experience and technical acumen developed therefrom
 
BR,
Shashank C Vagal 




From: Prasad Ghanekar <prs...@gmail.com>
To: material...@googlegroups.com
Sent: Saturday, 20 February 2016 10:12 AM
Subject: Re: [MW:24330] RE: 24309] PAUT & TOFD Level III

Reply all
Reply to author
Forward
0 new messages