weld joint configuration 20” Blind flange with 4” Weld neck flange

26 views
Skip to first unread message

Amul Raj

unread,
Apr 2, 2016, 3:32:19 AM4/2/16
to Materials & Welding

Dear Experts,


As per our project Design, an Isomeric Drawing given a weld joint configuration 20” Blind flange with 4” Weld neck flange (blind flange bored size 4”)

I never seen before this kind of weld joint configuration

But, our design engineer says that, there will not be any problem & it is acceptable. 

Please advise me where I can get the reference for this weld joint configuration

 

Regards,

Amul Raj T

Mohd Siraj

unread,
Apr 8, 2016, 12:15:38 AM4/8/16
to Materials & Welding
If it going to used as branch show them B31.3 brach joint configuration.