Re: P8 material limit of as per QW-403.6

189 views
Skip to first unread message

JAYAPAL DHAKSHNAMOORTHY

unread,
Dec 30, 2019, 12:35:07 AM12/30/19
to material...@googlegroups.com
  Dear experts,

I have qualified PQR of Thickness-6mm (P8G1) Austenitic stainless steel, & What is the minimum and max.thickness qualified  as Per QW-403.6.in WPS (for Impact).

Regards,
DHAKSHNAMOORTHY.J

Karthik

unread,
Jan 4, 2020, 10:07:20 AM1/4/20
to material...@googlegroups.com
Hi,
In your case it is 6mm thickness, Minimum qualified thickness is 3mm and maximum is 12 mm

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282SE-mail : karthi...@yahoo.com



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHHcqJdo7f3JVp4vAkH-77ucP9Gt4Z4uSVNmsM0o%3DfTr72cuXQ%40mail.gmail.com.

Brijesh Maurya

unread,
Jan 4, 2020, 10:07:20 AM1/4/20
to material...@googlegroups.com
As per QW-403.6, minimum base metal thickness qualified is T/2 i.e. 3mm & max. thk qualified is 2T i.e. 12 mm

JAYAPAL DHAKSHNAMOORTHY

unread,
Jan 5, 2020, 3:28:19 AM1/5/20
to material...@googlegroups.com
Hi Dears,

could you explain another also in QW 403.6 says (This variable does not apply when a WPS is qualified with a PWHT above the upper transformation temperature or when an austenitic or P.no.10H material is solution annealed after welding)


Regards,
DHAKSHNAMOORTHY.J

Hareesh K V

unread,
Jan 5, 2020, 9:12:43 AM1/5/20
to material...@googlegroups.com
Dear Sir, 

For the condition with impact testing,

The minimum thickness requirement is as per ASME BPVC Sec IX is 3 mm. 

The maximum thickness as per ASME BPVC Sec IX is 2T

But the maximum thickness as per ASME B 31.3 is T+6mm.

Regards, 

Hareesh K V


José Juan Jiménez Alejandro

unread,
Jan 5, 2020, 10:59:13 PM1/5/20
to material...@googlegroups.com
Good morning and greetings to all, dear colleagues and specialists on the subject.
You can cite the paragraph of ASME B31.3 where you specify that the maximum thickness is T + 6 mm, thanks in advance.



--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Hareesh K V

unread,
Jan 6, 2020, 3:17:32 AM1/6/20
to material...@googlegroups.com
Dear Sir, 

Please refer Table 323.3.1 of ASME B31.3.

Please review. 

Regards, 

Hareesh K V

ABHISHEK SINGH

unread,
Jan 13, 2020, 11:38:27 PM1/13/20
to Materials & Welding
As per QW-403.6 thickness limit will be 3 to 12 mm.
But in yours case what is the MDMT?

JAYAPAL DHAKSHNAMOORTHY

unread,
Jan 16, 2020, 10:17:24 PM1/16/20
to material...@googlegroups.com
Our MDMT is -45 degree

On Tue, 14 Jan 2020, 10:08 ABHISHEK SINGH <mech....@gmail.com wrote:
As per QW-403.6 thickness limit will be 3 to 12 mm.
But in yours case what is the MDMT?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

José Juan Jiménez Alejandro

unread,
Jan 16, 2020, 10:34:19 PM1/16/20
to material...@googlegroups.com

ABHISHEK SINGH

unread,
Jan 18, 2020, 8:59:22 PM1/18/20
to Materials & Welding
For P No. 8 impact test is not required for MDMT Minus 45 deg. C. It’s client requirement??