Hi all,
We qualified some welders to 6GR on 6" dia x 7 mm thick pipes using SMAW for root + hp (deposited about 4 mm) followed by FCAW. Now, if we want to use these welders for full SMAW - i) Is it allowed? ii) What is the new qualification to?
S Vagal |
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hi,
Sorry, the test coupon was 8"dia x 1/2" thick. My mistake. Root, HP - SMAW, Rest- FCAW.
Now, with this can the welder use SMAW alone to weld on some other joints within the Code ?
Hope I am eligible for an answer this time.
Thanks,
S Vagal
|
|
| Yes can weld SMAW alone ,but the thickness shall be within the qualified Range. Karthikeyan.S
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282 --- On Tue, 4/6/10, Shashank Vagal <nach...@yahoo.com> wrote: |
Thanks, Karthik.
Now, could you please give me a Code ref for this info? We always need to back what we say up with Code ref.
Appreciate your time and efforts,
|