Dears 
is allowed to generate a separate GTAW WPS from multi-processes PQR (GTAW+SMAW) as per EN15614-1. take into consideration that all PQR tests (bend, tension, hardness,...) had been carried out on the test coupon of PQR (combined processes


Bala Murugan

unread,
Nov 7, 2025, 11:32:11 PM11/7/25
to materials-welding
Hii..
Yes you can use it provided All essential and supplementary essential variables (if applicable) must be met for the individual WPS, just as they were for the PQR.

Thanks,
Balamurugan

On Sat, 8 Nov 2025, 8:15 am Left life, <life...@gmail.com> wrote:
Dears 
is allowed to generate a separate GTAW WPS from multi-processes PQR (GTAW+SMAW) as per EN15614-1. take into consideration that all PQR tests (bend, tension, hardness,...) had been carried out on the test coupon of PQR (combined processes


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGq5wx6VGW2Tx8Ru7dGVaypPdNNi7LOe%2B364q6e2WE3t%3DLqqvQ%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages