Material classification in AWS D1.1-reg

316 views
Skip to first unread message

Siva Chidambaram

unread,
Mar 3, 2015, 2:44:34 AM3/3/15
to material...@googlegroups.com
Hi friends,
 Kindly clarify my doubt.
 
In AWS D1.1, they have assigned groups for some materials.
I need to know whether we can use the Groups nos of the material if we are using the equivalent material of the assigned one in AWS D1.1 table 3.1.
 
For example. Material EN10025 S275 JR is not assigned in the Group of AWS D1.1 table 3.1. Whether I can assign it as Group 1, since its equivalent material is in Group 1 in AWS D1.1 Table 3.1
 
kindly clarify.
 
Thanks
 
M. Sivachidambaram
 

nithind...@gmail.com

unread,
Mar 4, 2015, 10:55:55 PM3/4/15
to material...@googlegroups.com
It comes under unassigned material and u have to go with separate PQR qualification for the same. Each unassigned material with its counter part material have to be separately qualified. However some clients accept it to use as group 1 or 2, without any requalifi cation. So take client concurrence.

Sent from my iPhone
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPJQpMVetV2ohFdAThXv_W-vKt7dRbx5u6KWE4349EgT_ZjU5A%40mail.gmail.com.