I am wondering if anyone knows what the maximum weave is for SMAW (specifically ASME Section VIII Div 1). For some reason 3x is sticking in my brain, but I would like to know where to find it in the ASME Codes. 

Kannayeram Gnanapandithan

unread,
May 21, 2016, 7:43:03 AM5/21/16
to materials-welding
u can find in PW40 also, it is 4Xcore dia not 3

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, May 21, 2016 at 12:58 PM, <haundpv...@gmail.com> wrote:
I am wondering if anyone knows what the maximum weave is for SMAW (specifically ASME Section VIII Div 1). For some reason 3x is sticking in my brain, but I would like to know where to find it in the ASME Codes. 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/24ee9b7d-4956-4f4d-8a40-86b41259ea8f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Chandra

unread,
May 22, 2016, 11:15:27 PM5/22/16
to material...@googlegroups.com
As per ASME Section VIII Div1, 
Please refer to the para UCS-56 (Requirements for Postweld Heat Treatment) para f(4)-a
Mentioned as maximum bead width shall be four times the electrode core diamter.

Best Regards,
Chandra

On 21-May-2016, at 2:28 PM, haundpv...@gmail.com wrote:

I am wondering if anyone knows what the maximum weave is for SMAW (specifically ASME Section VIII Div 1). For some reason 3x is sticking in my brain, but I would like to know where to find it in the ASME Codes. 

--

Chandra

unread,
May 22, 2016, 11:15:48 PM5/22/16
to material...@googlegroups.com
Please refer to ASME BPVC-1
PW-40.3.4 (d)
Electrode shall be four times the electrode core dia

Best Regards,
Chandra

On 21-May-2016, at 2:28 PM, haundpv...@gmail.com wrote:

I am wondering if anyone knows what the maximum weave is for SMAW (specifically ASME Section VIII Div 1). For some reason 3x is sticking in my brain, but I would like to know where to find it in the ASME Codes. 

--

John Henning

unread,
May 23, 2016, 10:50:46 AM5/23/16
to material...@googlegroups.com

Incorrect information.

 

First PW-40 is in Section I not Section VIII, so does not apply top question asked.

 

Second, PW-40.3.4 (d), which references bead width, applies only to repairs performed by the temper bead or half bead technique.  Very specialized application.

 

Third, there is no restriction otherwise on bead width in either Section VIII, Division 1, or Section I. 

 

One will often find such restrictions in customer specifications. 

 

Careful where you walk.  Free advice is worth just that.   

John Henning

unread,
May 23, 2016, 11:11:38 AM5/23/16
to material...@googlegroups.com

Again, incorrect information.

 

Section VIII, UCS-56.f.4(-a) applies only to repairs avoiding PWHT by use of temper bead or half bead technique.  See UCS-56.f.4(-c).

 

There is no weave width restriction for general welding in either Section VIII, Div. 1, or Section I.

 

Do not apply special case requirements to general welding.  A recurring mistake made by many.

dili...@gmail.com

unread,
May 24, 2016, 5:40:41 AM5/24/16
to John Henning
I fully concure

Sent from my BlackBerry 10 smartphone.
From: John Henning
Sent: Δευτέρα, 23 Μαΐου 2016 - 18:11
Subject: RE: [MW:24835] Weare or string

Reply all
Reply to author
Forward
0 new messages