Dear Experts,

Can anybody from our experts share some information regarding the below concern

As per ASME sec IX QW 451, the maximum thickness qualified for procedure is 2t up to 38mm thk for all materials, but for LTCS what is the maximum thickness range for procedure?


LTCS=  low temperature carbon steel. MDMT -10 deg celsius.


Thank you,
QA/QC Engineer,
Jay Poojary,
OCLLC Nigeria

S.Mohammed

unread,
Sep 6, 2015, 1:30:09 AM9/6/15
to Materials & Welding
What is basemtal thk.

Refer qw403.6 for base metal.range when impact applicable

t or 5/8t min..

george....@gr.bureauveritas.com

unread,
Sep 10, 2015, 8:48:41 AM9/10/15
to material...@googlegroups.com

is impact test a requirement?
What is the design and construction Code?

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Jay Poojary

unread,
Sep 10, 2015, 1:13:50 PM9/10/15
to material...@googlegroups.com
Dear Georgios sir,


 code applicable is ASME sec IX & B 31.3. Impact test required. please advice

cordially,
Jay Poojary

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/OFE168101B.F002AEC3-ONC2257EBC.004481A8-C2257EBC.00448CA8%40LocalDomain.

For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages