iHAVE A SCOOP TO WELD SOME ATTACHEMENT ON PIPELINE X52 
There any standard mention about welding attachement on pipe to follow or there also a special WPS AND PQR TO PREPARE 

TDK YOKESH

no leída,
23 nov 2020, 10:22:02 p.m.23/11/2020
para material...@googlegroups.com
Hi,
What kind of support are u welding?
B31. 8 does have some design requirement for welding attachments mostly the long seam fillet. There is some relation between the hoop stress to the SMYS constraints. 
V do support welding with low hydrogen as our spec calls for it. PQR with fillet fracture and macro ( to check the leg length and fusion) as per api 1104 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b91acd31-16e8-417a-b432-1ae6b9063073n%40googlegroups.com.
Responder a todos
Responder al autor
Reenviar
0 mensajes nuevos