I have a query regarding the minimum distance required between the toe of fillet weld to toe of girth weld, WPS being used as per AWS D1.1, since what I have in Aramco spec(SAES-W-013..Welding requirements for offshore structures) that distance between two butt weld joint's shall be maintain to 20 mm or 3 times of thickness of member, whichever is larger..

Thanks...

Hareesh K V

unread,
Apr 13, 2015, 10:54:05 PM4/13/15
to materials-welding

Dear sir,

In the case of distance between welds, in my opinion we cannot say a standard reference, what we usually does is, we follow the project spec. In your case also you can go with the same rule as of girth weld.

The logic behind the distance requirement is to avoid the overlap of HAZ.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/52643162-f8c3-4658-a9ca-599df4f27bd4%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Asif Raza

unread,
Apr 14, 2015, 7:12:39 AM4/14/15
to material...@googlegroups.com

Dear follow the Aramco Spec.

 

Peter

Welding Engineer

syed moinul hasan

unread,
Apr 17, 2015, 8:02:40 AM4/17/15
to material...@googlegroups.com
It all depend upon your project requirement.....As a thumb rule, it can be maintained 25 mm  gap .