please clarify below 

As per B31.3 above 16 mm ( P1 MATERIAL)thickness required PWHT?
what’s is minimum thickness required for PWHT as per B31.3 ( P1 MATERIAL)

Regard 
ELAVARASAN 


Hai Tran Ngoc

unread,
May 16, 2025, 12:44:08 AM5/16/25
to material...@googlegroups.com
According to B31.3
Table 331.1.1 PWHT
Table 331.1.3 Exemptions for mandatory PWHT

For nominal material thickness > 25mm not required PWHT if applied a preheat of 95 degree prior to welding.

For nominal material thickness > 5mm up to 25mm not PWHT required if applied multiple layer welds. (Single layer or single pass follow note 6 of table 331.1.3).

However, this depends by your WPS, if it is required by WPS you must be follow



 


Vào Th 6, 16 thg 5, 2025 lúc 09:35 Elavarasan Mech <elavaras...@gmail.com> đã viết:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yk4GW_Uq%2BhMu7hnqcq5NCEgu5%3D1ckMpLjLKZu2THbDKJQ%40mail.gmail.com.

Parminder Singh

unread,
May 16, 2025, 4:04:19 AM5/16/25
to material...@googlegroups.com
Dear Elavarsan 

As per B31.3

A preheat of 95°C (200°F) is applied prior to welding on any nominal material thickness >25 mm (>1.0 in.)
Multiple layer welds are used when the nominal material thickness >5 mm (>3 16 in.) [Single-layer or single-pass welds may be exempted from PWHT, provided the WPS has been qualified using single - pass welds with ±10%heat input and that all other conditions for exemption are met.]

Depends on Your WPS