NDT Procedure Level-III approval.

102 views
Skip to first unread message

chiluka venkatramulu

unread,
Jan 9, 2020, 4:09:02 AM1/9/20
to materials-welding
Dear All,
Pl clarify whether  it is required NDT Level-III approvals for all NDT procedures? or required only for coded vessels.
Pl specify the code requirement.

Thanks & Regards,
Venkatramulu CH

Kannayeram Gnanapandithan

unread,
Jan 9, 2020, 6:13:07 AM1/9/20
to materials-welding
Mainly required for stamp holders whether it is coded or non coded. All NDT procedure and personal are to be certified/ approved by Level 3. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdHdFX5ePVY4%2B5GB9pFh4ZGGoRu0ntafcZrkCw17XMdkrQ%40mail.gmail.com.

José Juan Jiménez Alejandro

unread,
Jan 10, 2020, 12:35:26 AM1/10/20
to material...@googlegroups.com
I have been in several ASME audits for recertification (Joint Review), with Designers U, S and R of the National Board, with the Authorized Inspection Agencies: OneCis and HSB GS and certainly non-Dstructive Testing Procedures are presented in these audits, such as VT, PT and others, and in none of the cases did these procedures carry signatures of a Level III of ASNT.
He estado en varias auditorias ASME para recertificación (Joint Review), con Designadores U, S y R del National Board, con las Agencias de Inspección Autorizadas: OneCis y HSB GS y ciertamente se presentan Procedimientos de Pruebas No Dstructivas en estas auditorias, como son VT, PT y otros más, y en ninguno de los casos estos procedimientos llevaron firmas de un Nivel III de ASNT.



--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





harenath jha

unread,
Jan 12, 2020, 11:16:43 PM1/12/20
to material...@googlegroups.com
It will be available in client specification

--