Dear experts,
Please let me know welder qualification range.
Details as below :
Actual Values
Pipe- Groove
1) P 43 To P 43 (SB-444)
2) GTAW ( Manual )
3) Thickness -5.54mm
4) SFA-5.14
5) F No- 43
6) Filler metal -ERNiCrMo-3
7) Position -6G
If I am not Wrong please check below i have mentioned Range Qualified.
Groove and Fillet Weld
1) P No - 1 thru 15F,34,41 thru 49
2) GTAW ( Manual )
3) SFA No- 5.xx
4) Thickness - 11.08mm
5) F no- 34,41,46
6) Filler metal - Any
7) Position - All
Please give me your feed back.
Regards
Kiran