Dear Experts,

I have a situation on structural member doubler plate welding.
We have to weld doubler plate welding with existing deck leg. During field survey we noticed that there is existing butt weld in deck leg, and doubler plate welding will be on top of same existing weld. Like welding on top of welding area. In that case we can flush grind existing butt weld and will do required NDT then proceed.

But is it code allowed welding on top of welding?

Srinivas.

harenath jha

unread,
Oct 9, 2019, 3:32:42 AM10/9/19
to material...@googlegroups.com
As per my understanding code is not stating any requirement for weld over weld .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f837a624-6e0d-4c6d-8655-3427153f152d%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages