Multiple welders can weld in a single production joint?

298 views
Skip to first unread message

Rajakani A

unread,
Jul 30, 2016, 2:38:09 AM7/30/16
to Materials & Welding
Dear friends,


 Can multiple welders weld in a single production joint in same process and position?

Kindly clarify me with reference ASME standards if any.

Regards,

Rajakani A,
L&T Construction,
Surat.

Mhaskar Aly

unread,
Jul 30, 2016, 10:33:56 PM7/30/16
to material...@googlegroups.com
Dear Rajakani...
It is allowed as there is no restriction from Code..Code is generally having restrictions...

hope to have your understanding..

Aly

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Hareesh K V

unread,
Jul 30, 2016, 10:34:52 PM7/30/16
to material...@googlegroups.com
Dear friend,

This can be done as there is no code restrictions. If the joint is failed all the welders are considered to be failed.

For bigger diameter pipes say, 60" which is usually welded by more than  one welder this can be accepted.

The concept of the production weld is to understand the ability of the welder in a real job situation. So on that basis try to avoid using multiple welders in one production joint.

Regards,

Hareesh K V 



Sent from my Samsung Galaxy smartphone.

dili...@gmail.com

unread,
Jul 30, 2016, 10:35:06 PM7/30/16
to Rajakani A
If they are qualified yes. It happens very often when ‎a welder performs root with GTAW and then an other completes with SMAW

Sent from my BlackBerry 10 smartphone.
From: Rajakani A
Sent: Σάββατο, 30 Ιουλίου 2016 - 09:38
To: Materials & Welding
Subject: [MW:25157] Multiple welders can weld in a single production joint?

--

Alan Denney

unread,
Jul 31, 2016, 6:38:09 AM7/31/16
to material...@googlegroups.com


For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

JIJILAL K M

unread,
Jul 31, 2016, 6:38:10 AM7/31/16
to material...@googlegroups.com
Please refer the attachment 

Best Regards,

JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand
#096 786 0129


--
production weld specimen.pdf

Hareesh K V

unread,
Jul 31, 2016, 8:33:27 AM7/31/16
to materials-welding

Dear Mr.Jijilal,

The pdf attachment  is production weld mockups for Procedure and performance qualification.

The production weld is the first joint  which  a welder welds after the qualification of his welder qualification test specimen.

Regards,

Hareesh K V


JIJILAL K M

unread,
Aug 1, 2016, 1:24:22 AM8/1/16
to material...@googlegroups.com
Mr. hareesh,
 You are right . the attachment shows this is the only instruction could find in code about production welding.
In many project i've qualified welders using production joints.

Best Regards,

JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand
#096 786 0129