Regarding weldability and properties of MS and 20MnCr5

311 views
Skip to first unread message

Sebastian Vettel

unread,
Jan 6, 2022, 5:15:10 AM1/6/22
to Materials & Welding
Please suggest the welding properties of mild steel, 20MnCr5 and EN19, and its procedure for TIG welding. Also please suggest which one would be better MS or 20MnCr5 considering the weight parameter.

Regards

dwh

unread,
Jan 9, 2022, 10:17:46 PM1/9/22
to material...@googlegroups.com, d...@btinternet.com

Has the component been case -hardened?

Aditya

unread,
Jan 10, 2022, 10:11:01 PM1/10/22
to Materials & Welding
No, not case hardened.

Devalkumar Desai

unread,
Jan 11, 2022, 1:06:23 AM1/11/22
to material...@googlegroups.com
Dear all, 

Plese advice better option for
Tubesheet:  SS 304L + Monel. 

1) Weld overlay . (Is possible??) 
2) Explosion Bonded. 

Br, 
Deval

On Mon, 10 Jan, 2022, 08:47 'dwh' via Materials & Welding, <material...@googlegroups.com> wrote:

Has the component been case -hardened?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2236ce4c.b5800.17e3ef143ac.Webtop.103%40btinternet.com.

Alcindo Jardim

unread,
Jan 11, 2022, 10:19:51 PM1/11/22
to material...@googlegroups.com
Depends of the sizes of the tubesheet...
Alcindo O. J. Jr.
21 96676-1511



dwh

unread,
Jan 11, 2022, 10:20:04 PM1/11/22
to material...@googlegroups.com, d...@btinternet.com

Hello,

Is the component part of the front-end assembly of a vehicle?

Is it a new component or a worn or damaged part that requires maintenance and repair?

Sincerely; 11 1 2022.

Aditya Sakhare

unread,
Jan 12, 2022, 4:08:18 AM1/12/22
to material...@googlegroups.com, d...@btinternet.com
Considering new component

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Kannayeram Gnanapandithan

unread,
Jan 17, 2022, 11:19:50 PM1/17/22
to materials-welding
Explosion Bonding

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Vinay Thattey

unread,
Jan 18, 2022, 10:17:45 AM1/18/22
to material...@googlegroups.com, dd10...@gmail.com
Dear Dev :
pl make it more clear   SS 304L + Monel

Reply all
Reply to author
Forward
0 new messages