Q235B equivalent

4,477 views
Skip to first unread message

Maroof Ali

unread,
Oct 29, 2010, 2:43:55 AM10/29/10
to material...@googlegroups.com
Dear friends

Chinese Q235B equivalent to which ASTM material?

Regards 

Maroof Ali

Karthik

unread,
Oct 29, 2010, 3:08:02 AM10/29/10
to material...@googlegroups.com

Hi,


Equivalent to CHINA STEEL STANDARDS - Q235B are as below


DIN17100-80 - St37-2


EN10025-2:1998 -  S235JR 


ASTM - A283 


JIS - SM400A


Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 10/29/10, Maroof Ali <maroofali...@gmail.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

V.S.

unread,
Oct 29, 2010, 4:38:00 AM10/29/10
to material...@googlegroups.com
Steel Specification
ASTM A36  
ASTM A53 B
ASTM A106 B
ASTM A131 B
ASTM A139 B
ASTM A381 Y35
ASTM A500 A
  B
ASTM A501  
ASTM A516 55
60
ASTM A524
 
ASTM A529  
ASTM A570 30
  33
  36
  40
  45
ASTM A573 65
58
ASTM A709 36


--