Dear experts,

while reviewing the material test certificates, I came across RAW material TC which is dated years back from the date of inspection of pipes which was ASTM A 105. and the RAW material TC does not shows A105 grade. its showing some other number. Pls clarify how I can make sure that it is the appropriate RAW material which is used for the manufacture of this pipe

Regards


Shankar Shivaratri

unread,
Apr 2, 2015, 1:23:38 AM4/2/15
to material...@googlegroups.com
A 105  related to forged rounds/fittings not not related to pipes please....

Thanks & Regards,
Shankar Shivaratri,
Hyderabad, India.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f39d79a8-443c-437a-8d72-5968d0526321%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Enrique roger Carrion Quinteros

unread,
Apr 3, 2015, 12:27:09 AM4/3/15
to material...@googlegroups.com

i think that you must be compared the physical and chemical propertys, and the  equivalent carbon.
Atte.
E carrion

Date: Wed, 1 Apr 2015 21:53:19 -0700
From: er....@gmail.com
To: material...@googlegroups.com
Subject: [MW:23031] Raw material certificate


Dear experts,

while reviewing the material test certificates, I came across RAW material TC which is dated years back from the date of inspection of pipes which was ASTM A 105. and the RAW material TC does not shows A105 grade. its showing some other number. Pls clarify how I can make sure that it is the appropriate RAW material which is used for the manufacture of this pipe

Regards



Reply all
Reply to author
Forward
0 new messages