IMPACT ASME SEC IX WPS/WQT

110 views
Skip to first unread message

Elavarasan Mech

unread,
Apr 7, 2025, 4:02:56 AM4/7/25
to material...@googlegroups.com
Dear Expert     
 we have qualified WPS for 8 mm  & 25 mm plate with impact (8-16 mm  range & 16-50 mm ) as per ASME sec IX 
What about the welder qualifications we need to be consider impact requirement same as per WPS or impact requirements doesn’t required for welder qualifications please guide me

Regards 
ELAVARASAN 

   



Deerendra Karanth

unread,
Apr 7, 2025, 5:14:34 AM4/7/25
to material...@googlegroups.com

QW-303.1 clearly states that “Welder performance qualification test need not include impact testing, even if the WPS requires it


Welder can be qualified without impact testing, as long as he welds a test coupon per the WPS.


But, you must ensure that the welder uses an impact-tested WPS when making production welds that require impact properties.

BR 

Deerendra 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4yma_rkksaAF0azyoL7jbiNNjZrp3taCiuHHWdumPT5mMg%40mail.gmail.com.

venkateswara reddy Desireddy

unread,
Apr 7, 2025, 5:14:41 AM4/7/25
to material...@googlegroups.com
Impact not a essential variable for welder, but welder must to follow WPS. 
Welder will get 2xdeposit material thickness.


Elavarasan Mech

unread,
Apr 7, 2025, 5:28:32 AM4/7/25
to material...@googlegroups.com
Thanks for the your reply 
we have qualified WPS for 8 mm  & 25 mm plate with impact (8-16 mm  range & 16-50 mm ) as per ASME sec IX  now I’m qualifie my welder 25 mm plate ( 5-50 mm range ) with and without impact doesn’t matter my interpretations is correct 



Regards 
ELAVARASAN


Manoj Mumbai

unread,
Apr 7, 2025, 6:19:17 AM4/7/25
to material...@googlegroups.com

Kannayeram Gnanapandithan

unread,
Apr 7, 2025, 9:25:35 AM4/7/25
to material...@googlegroups.com
WPS/PQR for Mechanical properties & Welding Performance Qualification for Welders is to verify his ability to make sound weld. Impact does not have any influences on welder performance.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Reply all