we have a CA6NM casting, we doubt there are repairs done by welding by supplier. what is the procedure to detect this detects by etching. 

If someone is having a procedure please share with me.

sincerely,
Abdulkadar Godil


safad pp

unread,
Apr 12, 2015, 11:19:20 PM4/12/15
to material...@googlegroups.com
Dear Abdulkadar ,

please refer ASME sec V111 div 1 ,non mandatory Appendix K.. Etch tests

Best Rgds.
Shafad P.P
ASNT Level III /AWS-CWI
Peekay Steel Castings(P) Ltd.,Calicut:India
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com.
> To post to this group, send email to material...@googlegroups.com.
> Visit this group at http://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/855f8efe-266b-4b8e-987f-b1489081063c%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages