How to prepare the test piece for IGC Test for filler wire and electrode...? where is given the detail about test piece preparation detail....

IGC TEST procedure as per  ASTM A262 PRACTICE-E


Thanks and regards
Sujit

Vishwas Keskar Welding Manager WELDING

unread,
May 2, 2023, 4:39:04 AM5/2/23
to Materials & Welding
Pl. ask Consumable supplier to issue CMTR . They will do testing and certify the batch with IGC Prac E 