Dear Experts,
We have a qualified PQR and WPS for Hardfacing overlay welding of Stellite 6 to C276 (UNS N10276; P-no.43 according to ASME IX QW-422)
The following applies to stellite:
CLASSIFICATION
AWS A 5.21: ER CoCr-A
EN ISO 14700: RZ Co2
DIN 8555: WSG 20-G0-40-CTZ
Used process: GTAW
Now the client wants us to do Ultimet hard facing overlay welding on Hastelloy C276.
For the Ultimet solid wired we found:
CLASSIFICATION
AWS 5.21: no class
UNS R31233
ASTM: B815
DIN: W.Nr. 2.4681
DIN CoCr26Ni9Mo5W
According to ASME IX, QW-432, all A5.21 is F-no.72 Filler wire
QUESTION:
Is it allowed to use above mentioned PQR (F-no.72 to P-no.43) to make a WPS for this job, or do we have to qualify a new PQR?
Looking forward to your valuable response,
Best regards,
Hans Smithuis
Valve Specialist / Welding Coordinator
Red Point Alloys BV email ha...@redpoint.nl
Radonstraat 2 phone +31 79 363 2070
2718 TA Zoetermeer website www.redpoint.nl
The Netherlands