WPS /PQR Approvel

66 views
Skip to first unread message

Santosh Patil

unread,
Oct 18, 2019, 7:02:12 AM10/18/19
to material...@googlegroups.com
Dear Members 


I have witnessed PQR of  SA312 TP 316 material 1" SCH 40  according to  Proposal WPS  , Test piece visually checked and send to Lab for check testing as per. Sec IX . also inform to vendor to be witness in Lab in the  presence of QC engineer . 
But vendor does not infirm to QC Engineer . and Lab test report is submitted . Now he pressurizes to approve WPS 
What shall I do..... 
S. B Patil

Dinesh Somwanshi

unread,
Oct 18, 2019, 7:29:09 AM10/18/19
to materials-welding
Dear sir, 

If it's NABL approved lab in India,  may consider for approval. 

For EIL approved jobs, May not possible to approve. 

Applicable to Indian client works only. 

Regards

Dinesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAETO-3tBgdsVjUKbeb6BcAFMP%3DkuaPkErfTXe76vYDtxP_O%2BFw%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Oct 18, 2019, 7:38:02 AM10/18/19
to materials-welding
is vendor stamp holder

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Venkatachalam Govindan

unread,
Oct 28, 2019, 5:32:40 AM10/28/19
to material...@googlegroups.com
If Lab is authorized by national, international (ISO/IEC 17025) or by the Client, you can review the parameters and you can approve.You should have adjustment there is no malpractice have done by both of them. You can also review any past experience with the lab and you can also go and witness the lab calibrations and qualifications, if everything OK then only you can make an NC for why there is communication gap happened? otherwise you can not reject the WPS unless there is any one suitable reason.

Just my opinion.

Best Regards,

Venkat. G



--
Venkatachalam Govindan
QHSE Lead / Trainer
(IRCA Registered Lead Auditor & API / CQI Practitioner)
+965 97604989, +919840502376 (
WhatsApp only)
Reply all
Reply to author
Forward
0 new messages