FILLER AND ELECTRODE AS PER THIS MATERIAL

118 views
Skip to first unread message

sujit kumar

unread,
Jun 5, 2022, 11:31:44 PM6/5/22
to Materials & Welding
Dear all
Good morning.
I want to qualify PQR for  SA516 GR 70  which electrode and filler wire i should use for that Qualification..??

sridh...@yahoo.com

unread,
Jun 6, 2022, 1:36:32 AM6/6/22
to material...@googlegroups.com

 

Dear Sujit Kumar,

SA 516 Gr. 70 is a low carbon fine-grain steel suitable for low temp. service. Heat input to be controlled to get good 
impact properties. 

The HAZ is roughly divided into three sections.

1.    The section adjacent to the weld shows a dendritic microstructure made of large pearlitic grains on a ferritic fund.

2.    The section in the middle shows a ferritic and pearlitic assorted grains of a similar size.

3.    The section apart from the weld shows ferritic and pearlitic grains on a fund of larger ferritic grains.

4.    The base metal, not affected by heat, remains the same, i.e. assorted pearlite and ferrite grains. 

SA 516 Gr, 70 is easy to weld using SMAW & GMAW if it is a plate. You can avoid using the GTAW process and this

process is generally recommended for root welding of CS, AS, and SS pipes and full welding of SS, AL, CU, Ni, etc. 

SMAW/GMAW/FCAW follows GTAW to economise the welding, where ever applicable or you can use SMAW all the

way up to cap pass or SMAW followed by SAW/ GMAW/ FCAW if the material thickness is 20-25 mm and above or

for higher volume production. 

Towards, consumable recommendation:

ER 70S-2 (with triple de-oxidizers) for GTAW root application and E 7018 for filler & cap passes (or)

E 7018 / E7016 for root, filler and cap passes.

ER 70S-6 for GMAW, E 71T-1 (or) E 70T-5 for FCAW and EL8 / EM12K for SAW processes. 

Pre-heating to 100-1500C and inter pass temp. are recommended for thickness above 20 mm.

Sridhar.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80a30ea2-d343-4b3d-9ea6-efedfca1a2a8n%40googlegroups.com.

Mohd Siraj

unread,
Jun 12, 2022, 11:23:41 PM6/12/22
to Materials & Welding
yes this material quite common to qualify P1G1/G2 qualification in one go!..
you can use ER70S-3 and E7018-H4R...with preheat/pwht applicale as per asme-ix.

Rameshbabu B

unread,
Jun 12, 2022, 11:40:28 PM6/12/22
to material...@googlegroups.com
For filler wire ER 70 S2
For electrode E 7018
For electrode with impact testing E 7018-1 shall be followed.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/80a30ea2-d343-4b3d-9ea6-efedfca1a2a8n%40googlegroups.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK’S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let’s come together as a nation so that they don’t have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

Kannayeram Gnanapandithan

unread,
Jun 13, 2022, 3:33:08 AM6/13/22
to materials-welding
What is the base thickness

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Srinivas Rao

unread,
Jun 14, 2022, 2:18:57 AM6/14/22
to Materials & Welding
Dear Sujith,
There are many filler wires/ elctrdoes  can be used for this material welding , 
we need to consider mainly application where this plate mateial will be used before selction the consuamble type /welding process to be used.

SMAW electrode selection based on joint type: Full penetration joint with single side welding :  E6013,E7016/ E7018/E7018-1(for MDMT: -29 & below applications) 
for double side weding or root by other process :  E7018/E7018-1 can be used
GMAW /GTAW: ER70S-2 up to -30 deg C & above impact applications&  ER70S-6 /ER80SNi-1is recommded up to -50deg C
FCAW: E71T-1/E71T-1C/E71T-1M  for  double side welding or root by other process  
SAW: EM12K/EH12K with recommended flux by different manufacturers. - doiuble side welding or root by other process 


Thanks & Regards,
Srinivas Rao
.