[MW:4950] Difference between densitostrip/step wedge calibration film/step wedge comparision film

54 views
Skip to first unread message

rutvik dixit

unread,
Apr 25, 2010, 2:35:36 AM4/25/10
to material...@googlegroups.com
HI all,
Is there any difference between densito strip and stepwedge calibration film and stepwedge comparision film? Your answer should be with reference to ASME SEC.V article 2

With Regards,
Rutvik
TATA Projects Ltd.


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.