RF pad clashing with circumferential pipe weld joints

115 views
Skip to first unread message

JIJILAL K M

unread,
Jul 30, 2016, 6:01:12 AM7/30/16
to material...@googlegroups.com
Dear Experts,

Refer to subject line and attachment , An RF pad is coming closely  with the circumferential weld of a lateral Tee.

Please advice how to resolve it. Code is ASME B 31.1.



Best Regards,

JIJILAL K.M. 
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand


HP STEAM RF PAD.pdf

Kannayeram Gnanapandithan

unread,
Jul 30, 2016, 6:51:10 AM7/30/16
to materials-welding
take RT on fouling area and extra area and u can close it 

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWb9xPp0KfV_gBBZh2Xu3Cm33QVuu8TjPAVW_SFmBUsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Hareesh K V

unread,
Jul 30, 2016, 10:34:31 PM7/30/16
to material...@googlegroups.com
Dear Sir, 

Take RT/UT of that area (consider the weld area of fillet weld for RF pad also)

After getting it cleared in RT/UT; flush grind the area and do the fitup of the RF pad.

Some specification insists to do DPT after flush grinding (Even after acceptance of RT/UT); before fitup of RF pad.

Regards,

Hareesh K V



Sent from my Samsung Galaxy smartphone.

raneesh pk

unread,
Aug 1, 2016, 1:24:22 AM8/1/16
to Materials & Welding
Dear Jijil,

Take RT of the  circumferential joint and before  pad fit up flush the joint area  and if need DP to be carried out 
Reply all
Reply to author
Forward
0 new messages