Indication on RT after Clad Weld Overlay-625

123 views
Skip to first unread message

israr ahmed

unread,
Dec 14, 2014, 4:15:13 AM12/14/14
to material...@googlegroups.com
Dear Friends,

Could you Pls inform me about the attached RT film Photos are acceptable?
If acceptable or not acceptable which code I should Ref. 

The indications are found after cladding 
--
Israr Ahmed Noor Mohammed
+919930308261
IMG_20141213_111821.jpg
IMG_20141213_111850.jpg
IMG_20141213_112825.jpg

Agu Didie

unread,
Jan 12, 2015, 9:25:41 PM1/12/15
to material...@googlegroups.com
dear israr,

may i know what this type of material? piping, structure or etc? details pls.

Shashank Vagal

unread,
Jan 13, 2015, 11:50:34 AM1/13/15
to material...@googlegroups.com
Please attache the image.......
 
With Best Regards,
Shashank C Vagal

From: Agu Didie <didi...@gmail.com>
To: material...@googlegroups.com
Sent: Tuesday, 13 January 2015 7:55 AM
Subject: [MW:22716] Re: Indication on RT after Clad Weld Overlay-625

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/890d71e8-f996-4a9c-b401-28cc2ece4936%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Neilashkumar

unread,
Jan 14, 2015, 2:13:36 AM1/14/15
to material...@googlegroups.com
  Dear all,

We have a project for Seam Welding repairing work of Stainless steel
round duct piping for rubber finish building,details are as follows,
Total repairing welding length-500-550meter
Pipe material.    --EFW304/304LSS A240
Pipe thickness --below 3mm
Pipe size --0.75" -20"dia
Can you please tell me whether it is possible to do repair welding ? Method
to do repair weld.

P.NEILASHKUMAR
Sent from my iPad
MOB : 966 533098265
           91+9952110791


Shomenath Bagchi

unread,
Jan 14, 2015, 2:58:18 AM1/14/15
to material...@googlegroups.com
We may have to check the actual extent/ condition of damage in welds to evaluate the repairing possibilities.

S.N.Bagchi.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

c sridhar

unread,
Jan 16, 2015, 11:05:53 AM1/16/15
to material...@googlegroups.com
In principle Possible. U can use pulsed TIG welding process with  same type
filler wire and  a lower size.

But u have not mentioned the type of defect in the weld for better guidance.
 
C Sridhar.

Please don't print this e-mail unless you really need to. Save the environment.




 


From: 'Neilashkumar' via Materials & Welding <material...@googlegroups.com>
To: "material...@googlegroups.com" <material...@googlegroups.com>
Sent: Tuesday, 13 January 2015 11:44 PM
Subject: [MW:22721] Thin material welding

Neilashkumar

unread,
Jan 16, 2015, 11:24:17 AM1/16/15
to material...@googlegroups.com
Welding done with seam welding process  and found lack of fusion ,visual is rejected. Now the client is insist us too do repair welding and the joint should be full penetration weld according to ASME B31.3 seam welding.
Since it is 3mm thick material we need to do high travel speed welding , can we use GMAW -STT  process?


P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 535017935
            91+9952110791

Raju Kandula

unread,
Jan 20, 2015, 11:06:25 AM1/20/15
to material...@googlegroups.com
Indication shows as gap between cladding materials due to incomplete fusion or penetration

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages