The FCAW Gas Shielded process shall not be used for the root pass on full penetration, groove joints that are welded from one side only without backing
The FCAW self-shielded shall only be permitted prior approval through pWPS with full matrix of proposed testing
Thanks and Regards
Rameshkannan Devaraj
"What you have learned is a mere handful; What you haven't learned is
the size of the world – Avvaiyar"
Kindly advice
in general major clients write in thier specs FCAW process not allowed in presure vessel & pressure pining joints
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/926b0970-558d-47f7-8c53-3de21d008787%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcGnn%3DKfEiXm_vD6wnuP-czLfiYKPwhbPr8k3b9sPPfO1Q%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcGnn%3DKfEiXm_vD6wnuP-czLfiYKPwhbPr8k3b9sPPfO1Q%40mail.gmail.com.