Regarding Fillet weld WPS (for less than 5mm thk)

93 views
Skip to first unread message

Rejoy Thomas

unread,
Aug 13, 2019, 11:23:48 PM8/13/19
to material...@googlegroups.com
Dear all,
            Can I weld a socket/fillet joint, where the thickness of base metal (pipe to half coupling) is less than 5mm, by using a WPS which is qualified for 5-50mm thickness (GTAW+SMAW, P1 to P1), since there is no groove/base metal thickness involved in fillet welds!! Kindly refer the clause during reply. Your earliest response would be highly appreciated!!

Thanks & Regards

Rejoy Thomas

munee...@gmail.com

unread,
Aug 14, 2019, 7:50:49 AM8/14/19
to materials-welding
Go ahead per 452.6-Table-IX-ASME...

Thanks...
Muneeb
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc278%2BDqB-e2PgNcmT0VjBtDQmjnHuuvUPoNbJipaMue8%2BLg%40mail.gmail.com.

Karthik

unread,
Aug 14, 2019, 7:50:49 AM8/14/19
to material...@googlegroups.com
Hi,
Yes. You can use for all fillet sizes on all base metal thickness. See below.

Inline image


Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthi...@yahoo.com



--

munee...@gmail.com

unread,
Aug 15, 2019, 12:43:56 PM8/15/19
to materials-welding
Yes, check procedure for QW-451.4 / performance for QW-452.6.

Hence go ahead for both procedure / performance.

Thanks
Muneeb