Dear experts,

I am qualifying 2 welder on 20" pipeline. One half welder by welder A and other half welder B.  The RT result shows Welder A side failed and Welder B side passed.
Query : Both the welders are rejected as the coupon has failed or should I consider welder A and welder B passed.

Any code reference or interpretation on similar case will be helpful. 

Vaishakh Kc

unread,
Mar 17, 2021, 11:07:46 PM3/17/21
to material...@googlegroups.com
Which code permits to do wpq like this?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuovOFQLQmMRN17eosER4WP1cMtcEWQb%2BRhiAnvmaEG7EA%40mail.gmail.com.

pgos...@rogers.com

unread,
Mar 17, 2021, 11:50:19 PM3/17/21
to material...@googlegroups.com

Hi TKD Yokesh,

 

I believe this requirement included in API 1104, 2020 edition, clause 6.1, which is still in the draft stage, not yet approved and published. This means this Code is yet to be a legal document. I did not see this clause being mentioned in 2018 or earlier versions.

Anyway, the answer to your query is as below. This sounds sensible , when each welder is welding half- circumference of the pipe. That’s not the case when 2 welders weld on the same coupon, each of them welding the entire circumference.

 

Thanks.

 

 

 

Pradip Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

image003.png

TDK YOKESH

unread,
Mar 18, 2021, 12:26:48 AM3/18/21
to material...@googlegroups.com
Hi Pradip Sir , 

Appreciate your answer on this subject . Hope this clause shall provide a straight answer to people who have this concern of misinterpreting the code . We have cases where people  expect a direct answer to this kind of question in code . 

Thanks a lot .

image003.png

Raghuram Bathula

unread,
Mar 18, 2021, 12:36:12 AM3/18/21
to Materials-Welding
Pl refer interpretationimage.png
image.png

TDK YOKESH

unread,
Mar 18, 2021, 1:28:35 AM3/18/21
to material...@googlegroups.com

Dear Raghuram Sir , 


Thanks  for your information . Appreciate if you share the latest interpretation of API 1104 as I am unable to find the API-I-1119 -19 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--

Best regards,

TDK YOKESH

PH : +917092847368


Reply all
Reply to author
Forward
0 new messages