UT OF PARTIAL PENETRATION JOINT OF STRUCTURAL WELD

276 views
Skip to first unread message

asad azmi

unread,
Apr 4, 2011, 1:25:09 PM4/4/11
to material...@googlegroups.com
Dear All,
 
Greetings....
 
Is it possible to perform UT of  Partial Penetration weld joint of beam with base plate.
 
construction code is AWS D1.1.
 
Thanks and Regards 

Kale, Bhaskar M

unread,
Apr 5, 2011, 12:08:52 AM4/5/11
to material...@googlegroups.com
yes ,no problem for that, what is the thickness and what is the purpose of examination to check penetration or weld quality?
regards, Bhaskar

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

muthusrinivasan muthuselvam

unread,
Apr 5, 2011, 6:46:45 AM4/5/11
to material...@googlegroups.com
Yes it is possible..
 
You can ensure the depth of fussion & root fussion(if required)
 
best regards,
 
msms
 


 
--