Dear All
Can you advice, 
two weld  joint how much Min distance between weldjoints.
Please clarify, if possible please provide code reference.

Best regards

Guru

Hernan Arturo Castillo Mier

unread,
Oct 4, 2019, 7:33:17 AM10/4/19
to material...@googlegroups.com

Hello:

 

 

 

 

 

 

 

Hernán Castillo Mier

Ingeniero Senior Confiabilidad e Integridad

FACILITADOR AUTORIDAD TÉCNICA EQUIPO ESTÁTICO

INSPECTOR AUTORIZADO

API 510 (33119)

Avantel: 8*1571

Teléfono: 668-2396

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEDN%2BXFp1f7duhV4NFBmu_87QNzsuA877q4wDUTDuEOPTOM7eQ%40mail.gmail.com.

Este mensaje puede contener información de tipo personal, clasificada o reservada; si usted no es el destinario, por favor, hacer caso omiso de su contenido y abstenerse de compartirlo, reenviarlo o copiarlo. Si recibe este mensaje por error, agradecemos informarlo inmediatamente al remitente y borrarlo permanentemente de su cuenta. Si usted está autorizado para recibir la información de tipo personal, se le recuerda que esta información debe ser manejada con la finalidad con la que ha sido solicitada y en virtud de la normativa que habilita el acceso a la misma. Así mismo, deberá ser usada bajo los parámetros de la ley 1581 de 2012 de protección de datos personales y la normativa que la desarrolla, siendo responsabilidad del área receptora del cumplimiento de la citada normativa de protección de datos personales. CONFIDENTIALITY NOTICE: This electronic transmission (including any files attached hereto) (this "Communication") contains information that is or may be legally privileged, confidential, and exempt from disclosure without our express permission in advance. The information is intended only for the use of the individual or entity named above. If the reader of this message is not the intended recipient or any employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any disclosure, dissemination, copying, distribution, or the taking of any action in reliance on the contents of this electronic Communication is strictly prohibited. If you have received this Communication in error, please notify the sender immediately and destroy permanently the transmitted information in its entirety and do not disclose its contents to any other person. Para conocer la Declaración de Tratamiento de Datos Personales de Ecopetrol, favor consultarla en www.ecopetrol.com.co Responsabilidad Corporativa – Declaración de Tratamiento de Datos Personales.

Kannayeram Gnanapandithan

unread,
Oct 5, 2019, 4:02:16 AM10/5/19
to materials-welding
Ref BSEN 15952-5

Adam Janzeer

unread,
Oct 6, 2019, 11:40:43 PM10/6/19
to material...@googlegroups.com
Dear ALL 

As per my knowledge, It's a good engineering practice mostly highlighted on our project specification or client procedure.
For your reference refer below clause extracted from SHELL DEP 31380131

3.3 ASSEMBLY OF PIPING COMPONENTS
For butt-welding of all piping components (e.g. pipe ends, fittings and welding neck
flanges), a uniform root gap shall be provided as specified in the relevant Welding
Procedure Specification.
Flange bolt holes shall straddle the vertical centerline of the pipe where the flange is
installed vertically, and the north-south line where the flange is installed horizontally.
Refer to DEP 31.38.01.11-Gen. for flange misalignment acceptance criteria of misalignment
of flanges.
The minimum distance between the edges of two pressure-containing welds shall be twice
the wall thickness of the thicker pressure part. The same requirement applies to the
distance between non-pressure attachment welds and a pressure-containing weld in order
to allow non-destructive inspection of the pressure-containing weld.



Longitudinal welds in two adjacent pipes should be 180° apart, but in any case shall be separated
by at least twice the wall thickness of the thicker pipe. When pneumatice leak test in accordance
with ASME B31.3, para. 345.4 is performed in lieu of hydrostatic leak test, the minimum spacing of
the longitudinal welds SHALL [PS] be followed.

If the pipe contains a longitudinal weld, this weld SHALL [PS] not be located at the bottom of the
pipe after installation; it should be located at least 45° from the bottom of the pipe.



Maha Charu

unread,
Oct 6, 2019, 11:42:11 PM10/6/19
to material...@googlegroups.com

mohsin tufail

unread,
Oct 9, 2019, 2:18:17 AM10/9/19
to material...@googlegroups.com
20mm or three times of the wall thickness which is greater

Adam Janzeer

unread,
Oct 9, 2019, 3:32:42 AM10/9/19
to material...@googlegroups.com
Dear moshin

Based on which reference....

mohsin tufail

unread,
Oct 9, 2019, 11:14:46 PM10/9/19
to material...@googlegroups.com
reference aramco standard w-11 
11.1
The minimum distance between parallel butt welds shall be 20 mm or 
three times the wall thickness of the joint, whichever is greater

atul khatri

unread,
Oct 10, 2019, 1:57:31 AM10/10/19
to material...@googlegroups.com
Dear Siva,
You must be aware that min. separation distance between two welds is to isolate there heat affected zone (HAZ).
HAZ depends on so many factors out of which thickness is the key one.
So as Mohsin and Adam suggested, these requirements are mainly guided by client's specifications based on their practical experiences or lesson learnt. 
So you could take gap between two welds as maximum between 50 mm (based on good engineering practice), twice the wall thickness of the thicker pressure part (As Adam advised) and 20 mm or three times the wall thickness of the joint (as Mohsin advised).
If you go with the above for sure you will not face any issue.
Also take note that if you are asking about the weld joints for piping spool, it will be good to have the minimum spool length as equal to pipe nominal diameter for 6" and above and for lesser size it should be 100 mm. 

Thanks

Kannayeram Gnanapandithan

unread,
Oct 10, 2019, 4:35:23 AM10/10/19
to materials-welding
As per DIn EN 12952-5,(2012) 8.1.7. should be greater than 40mm

Paidi

unread,
Oct 11, 2019, 1:42:37 AM10/11/19
to material...@googlegroups.com
Dear Shiva

Please see your project specification ....Distance between weld join will varies as per Client standards... 

In general ..3 times of WT should be required ...

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEDN%2BXFp1f7duhV4NFBmu_87QNzsuA877q4wDUTDuEOPTOM7eQ%40mail.gmail.com.


--
Thanks  & Best Regards,

Suresh Paidi


 
Reply all
Reply to author
Forward
0 new messages