What is the best guide to ASME Sec IX?

428 views
Skip to first unread message

Johnson Madukayil

unread,
Jun 14, 2009, 7:35:54 AM6/14/09
to material...@googlegroups.com
Friends,

Can you please tell me as to what is the best guide to learn to apply ASME Sec IX other than on the job training?

Regards

Johnson

endri.p...@gmail.com

unread,
Jun 14, 2009, 7:51:08 AM6/14/09
to material...@googlegroups.com
Hi Johnson,

I suggest you to learn first welding engineering, material science prior to apply this code. It will be helpful rather than you learn it without any basic.

Regards,
Endri

Powered by Telkomsel BlackBerry®


From: Johnson Madukayil
Date: Sun, 14 Jun 2009 07:35:54 -0400
To: <material...@googlegroups.com>
Subject: [MW:2431] What is the best guide to ASME Sec IX?

Johnson Madukayil

unread,
Jun 14, 2009, 7:51:05 AM6/14/09
to material...@googlegroups.com
I am familiar with welding engineering and material science and am currently working as a Sr. Design Engineer in a Nuclear Power Plant with over 10 years of ASME Sec VIII and III experience.

Thanks

Johnson

Ali Asghari

unread,
Jun 14, 2009, 7:53:27 AM6/14/09
to material...@googlegroups.com
hartford publication has a guide that it is very complete & easy to understand.


From: Johnson Madukayil <jmadu...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, June 14, 2009 4:05:54 PM
Subject: [MW:2431] What is the best guide to ASME Sec IX?

rajeev arora

unread,
Jun 14, 2009, 8:18:24 AM6/14/09
to material...@googlegroups.com
ali
can you give some refernce or name of the Guid book and availablty location wise?


 
2009/6/14 Ali Asghari <asgha...@rocketmail.com>
--
Regards

Rajeev Arora




"DON'T LET SOMEONE BECOME A PRIORITY IN YOUR LIFE...
WHEN YOU ARE JUST AN OPTION FOR THEM....."

SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,

welding_...@charter.net

unread,
Jun 14, 2009, 9:26:09 AM6/14/09
to material...@googlegroups.com
A good guide is CASTI's http://www.casti.ca/ CASTI Guidebook to ASME
Section IX - Welding Qualifications

Richard Beldyk, PhD, PE

Original Message:
-----------------
From: Johnson Madukayil jmadu...@gmail.com
Date: Sun, 14 Jun 2009 07:51:05 -0400
To: material...@googlegroups.com
Subject: [MW:2434] Re: What is the best guide to ASME Sec IX?


I am familiar with welding engineering and material science and am currently
working as a Sr. Design Engineer in a Nuclear Power Plant with over 10 years
of ASME Sec VIII and III experience.

Thanks

Johnson

On Sun, Jun 14, 2009 at 7:51 AM, <endri.p...@gmail.com> wrote:

> Hi Johnson,
>
> I suggest you to learn first welding engineering, material science prior
to
> apply this code. It will be helpful rather than you learn it without any
> basic.
>
> Regards,
> Endri
>
> Powered by Telkomsel BlackBerry®
>
> ------------------------------
> *From*: Johnson Madukayil
> *Date*: Sun, 14 Jun 2009 07:35:54 -0400
> *To*: <material...@googlegroups.com>
> *Subject*: [MW:2431] What is the best guide to ASME Sec IX?
> Friends,
>
> Can you please tell me as to what is the best guide to learn to apply ASME
> Sec IX other than on the job training?
>
> Regards
>
> Johnson
>
>
>
> >
>




--------------------------------------------------------------------
mail2web.com – What can On Demand Business Solutions do for you?
http://link.mail2web.com/Business/SharePoint


Arunachalam A

unread,
Jun 14, 2009, 9:54:47 AM6/14/09
to material...@googlegroups.com
I am sorry, I have misplaced.
I will send as soon as I get the same.
 
I have an old  casti filler metal handbook, which may be of some use to you.
arun

On Sun, Jun 14, 2009 at 5:00 PM, Arunachalam A <arun...@gmail.com> wrote:
I will send you a CAST Guide book for section IX.
arun

--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==



--
ARUNVANI

Smiling Opens the Heart

Good feelings for others are like ointments that heal wounds and re-establish friendships and relationships. Good feelings are generated in the mind, are transmitted through your attitude and are reflected in your eyes and smile. Smiling opens the heart and a glance can make miracles happen.

SMILE IS A COOLING SYSTEM OF HEART,
SPARKLING SYSTEM OF EYES, LIGHTING SYSTEM OF FACE, RELAXING SYSTEM OF MIND....
SO TO ACTIVATE ALL YOUR SYSTEM
==ALWAYS KEEP SMILING==
BlueBookLite.pdf

Sadique Sheikh

unread,
Jun 15, 2009, 9:24:50 AM6/15/09
to material...@googlegroups.com
I have attached here the CASTI GUIDEBOOK for understanding ASME section IX.

Regards
M. SADIQUE