Missed one of information,
Rail section welding done by Mobile Flash Butt Welding Machine- Automatic.
Regards,
Dear Experts,
I am new in this group and very glad to see conversation regarding needfull and got required answer of any issues.
Now, I have facing one of issue, At present working with Indian railway project, thirt party is also there from client side. They does't know what the wps & pqr becoz. Wps & PQR is not mentioned in their spec./manual. But as per IS standard testing they have carried.
But 2nd authority is saying make wps & pqr.
Now question is... whats the parameter to be set for rail section? Because all parameter are different from piping or structure. Whats format as per section IX or ...?
Mat. Spec. .. IR T12 grade 880, 60kg 90 uts
Requesting all of you, Please advice and send a sample wps & pqr as per this mat. Spec.Regards,