Re: Verticality tolerance required for steel chimney as per code.

895 views
Skip to first unread message

Ramesh Meka

unread,
Jan 4, 2014, 8:13:08 AM1/4/14
to materials-welding
Dear All,
Can any body provide Verticality tolerance required for steel
chimney as per code and also send applicable code. Thanks in advance.

--
Thanks & Regards,

M.Ramesh,
Mob.+918456805540.

*Please consider the environment before printing this email.*

veera raghava kommisetti

unread,
Jan 4, 2014, 11:30:51 PM1/4/14
to material...@googlegroups.com
Chimeny is for which application??
for guidence i am attaching API 560 std (chimeny for fired heaters)
 
 
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

API 560.xps

Muthu Samy

unread,
Jan 4, 2014, 11:07:58 PM1/4/14
to material...@googlegroups.com


1mm in 1 m as per AWS D 1.1

வாழ்க வளமுடன் என்றும் நலமுடன்

LOVE EVER HURT NEVER

Muthusamy.S

அமீரகம் 






GENE MATSKO

unread,
Jan 4, 2014, 11:18:36 AM1/4/14
to material...@googlegroups.com
Check  IS 6533, Part 2, Code of Practice for Design and Construction of Steel Chimney. 
Gene Matsko


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

Karuppan

unread,
Nov 6, 2017, 6:01:20 AM11/6/17
to Materials & Welding
Dear
The vertical tolerance for steel chimney is H/600. As per the International committee on Industrial chimney.
Karuppan.P
Nuberg engineering limited.