PQR Test coupon diameter range. Can i qualify in 2 Inch NPS? ASME sec 9

793 views
Skip to first unread message

Srinivas Engr

unread,
Mar 4, 2011, 1:50:08 AM3/4/11
to Materials & Welding
Dear All,

As per QW 310, the test coupon sizes shall be NPS 6 inch or greater?
for PQR & WPS qualification, can i go with NPS 2 inch test coupon?
(possible r not)
if i do witt 2 inch then how many test coupon i want to make?

Regards
srinivas

Karthik

unread,
Mar 4, 2011, 1:57:41 AM3/4/11
to material...@googlegroups.com
Hi,
You can go with 2" coupon.But you should also consider whether Only one 2" test coupon is enough for all mechanical test to be done.If the test specimen is not enough for mechanical tests,you should do aditional one coupon for sufficient mechanical test specimens.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 3/4/11, Srinivas Engr <srinivas...@gmail.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

atul chaturvedi

unread,
Mar 4, 2011, 1:50:33 PM3/4/11
to material...@googlegroups.com
Dear Sriniwas,

QW-310 is for Welding performance qualification not for WPS / PQR. Diameter is not consider (variable) for WPS / PQR.                                     

You can use plate or pipe (Any diameter) for WPS / PQR.

Regards

Atul chaturvedi