Wrapping and Coating Procedure for Cooling water Buried CS Piping.

23 views
Skip to first unread message

chiluka venkatramulu

unread,
Dec 9, 2021, 1:09:11 AM12/9/21
to materials-welding
Dear All,
Pl can anybody provide the Wrapping and Coating Procedure  for Cooling water Buried CS Piping with applicable specks.

Thanks and Regards,
Venkatramulu CH

vishal hirde

unread,
Dec 9, 2021, 4:03:42 AM12/9/21
to material...@googlegroups.com
Dear Venkant,

Kindly refer AWWA C203 :AWWA Standard for Coal-Tar Protective Coatings and Linings for Steel Water Pipelines - Enamel and Tape - Hot Applied

Regards,

Vishal

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdE%3DrhpqGYD6NPmF%3DOA8MiH-QcHWYYWGC%3D%2Bf6ENyJNwT7w%40mail.gmail.com.



Reply all
Reply to author
Forward
0 new messages