Mill tolerance as per ASME

626 views
Skip to first unread message

Rishabh Chandnani

unread,
Nov 7, 2021, 10:58:56 PM11/7/21
to material...@googlegroups.com
Mill tolerance for the seamless pipe is 12.50% and 0.3mm for the welded pipe.

Whereas Mill tolerance for the seamless/welded fitting & flange  is 12.50% 

Is standard more stringent in case of welded pipes ?

Please justify.

Regards
Rishabh

Mhaskar Aly

unread,
Dec 9, 2021, 11:09:28 PM12/9/21
to material...@googlegroups.com
Tolerances are set based on manufacturing process.

Welded pipes, there is very less chance of thinning so is the tolerance. Cut from coil and rolled and welded.

Further 12.5% mill tolerance is considered while designing the item, and so thickness of pipe will be design thickness plus mill tolerance plus Corrosion allowance.

Mhaskar Ali 
Dubai 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFH_NRKqdyNRYK3bwDnKgd%2BUBHaXDQF6o1WMVfkhTNxNJrNEpw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages