Change of NDT in repairs joint

66 views
Skip to first unread message

Prasad Rode

unread,
Mar 27, 2017, 8:31:30 AM3/27/17
to Materials & Welding
Dear sir,

Is it allow to change the NDT method, while checking the repaired weld joint.
For example: we do the radiography of weld joints, then after repaired in some joint, due to some reason, we are performing UT.

Is it allow us or not, to accept that repaired weld joint on the basis of UT.

Hoping for valuable advice.

Regards
Prasad

dilintas

unread,
Mar 28, 2017, 10:14:59 AM3/28/17
to material...@googlegroups.com
ASME Code Sections allow substitution of RTS by UT only under specific conditions but not on your case



Sent from my Samsung Galaxy smartphone.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d70ed22-4a56-419e-9b19-c58fb6a6b075%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Perumal Govindan

unread,
Mar 28, 2017, 11:22:00 AM3/28/17
to material...@googlegroups.com

Hi

It is possible only if the Client or project Specification permits.

Regards
Govindan Perumal

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

M.Sathiya Narayanan

unread,
Mar 29, 2017, 11:16:19 PM3/29/17
to material...@googlegroups.com
based on client approval

Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d70ed22-4a56-419e-9b19-c58fb6a6b075%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards
M.Sathyanarayanan

Prasad Rode

unread,
Mar 29, 2017, 11:17:50 PM3/29/17
to Materials & Welding
Dear sir,

1) Means it is not allow to do any change in NDT method for repair acceptance of weld joint.


2) But asking only for information and discussion that , why is it not allow as my NDT changing or replacing method is equivalent to first one?

UT and RT are volumetric NDT method.

Regards
Prasad

Dinesh Somwanshi

unread,
Mar 30, 2017, 1:33:33 AM3/30/17
to materials-welding
Dear sir,

Its not allowed in API standard as well. The process of NDT should be same on repair joint also verify or start from intial stages. 

*DINESH VITTHAL SOMWANSHI*

*BACHELOR IN MECHANICAL ENGINEER*

*AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL,*
*API 570 - Piping Inspector,** AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3*
*NDT II -UT , RT , MT , PT, VT*
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*



Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Prasad Rode

unread,
Mar 30, 2017, 11:21:13 PM3/30/17
to Materials & Welding
Dear sir,

Asking as information only,
is it written/mentioned anywhere in code like API, that it is not allowed to change the Ndt method or only same has to used.



Regards
Prasad