Dear Experts,

We are working for a client with ASTM 588 grade B material which is atmospheric corrosion resisting steel.
With SMAW and ASW E 8018 W2 electrode.

We are facing distortion problems -  bend / tilt, while fabricating of I beam structures.

Even after giving adequate supports distortion happening. 
'
My question is is by heating the job and rectification is the only process OR cold pressed rolling is advisable for this material.

Please advice.