WPS & PQR for P8-P1 and P8-P8 as per ASME Sec.IX

402 views
Skip to first unread message

SANJAY SINGH

unread,
Feb 29, 2024, 5:40:42 AM2/29/24
to material...@googlegroups.com
Dear Experts ,
            Can anyone suggest my below queries
1. I have WPS and PQR with P8 to P1 Base metal  Grade 316 to E250 BR then can I use this PQR for SS304 Grade base metal welding .
2. Similarly I have P8-P8 WPS , PQR in Grade SS316 then can I use this PQR for the welding of SS304 base metal.

Pls. suggest .

Regards 
S.R.Singh

Parminder Singh

unread,
Feb 29, 2024, 7:49:31 AM2/29/24
to material...@googlegroups.com
Dear Sanjay

Yes you can use, but subject to : 
1. No Charpy Impact Test requirements 
2. No Heat Treatment requirements

Thanks 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALkBf%2Bvy_kF3j1y74J5pGKcVhMfvCaeEUk%2BCNA8hUd%2B9-Lab%3Dg%40mail.gmail.com.

Hai Tran Ngoc

unread,
Feb 29, 2024, 7:49:41 AM2/29/24
to material...@googlegroups.com
No, because they are produced with different standards.
SS304 & SS316 refer to JIS standard
Materials related to P1 and P8 refer to ASME Sec II Part A and ASTM standards.
According to ASME Sec IX, the above issues are essential variables.


Vào Th 5, 29 thg 2, 2024 lúc 17:40 SANJAY SINGH <sanjay.k...@gmail.com> đã viết:
--

Vinay

unread,
Mar 23, 2024, 10:17:19 AM3/23/24
to material...@googlegroups.com
Dear Sanjay ..E250BR is SA-36 . You have a WPS/PWR  for P1-P8 ..You can not use it for P8 -P8.             U can use P8-P8 PWR for SS 304

--