Low alloy steel Golden joint root NDT

103 views
Skip to first unread message

Karuppa Samy

unread,
Oct 21, 2024, 2:48:14 AM10/21/24
to material...@googlegroups.com
Dear All,

How can we do root NDT for low alloy (HS service) steel golden, while doing continuous preheat ( 300°C) and can you recommend suitable NDT methods.

Regards
K. Karuppasamy,



sridhar cn

unread,
Oct 21, 2024, 9:08:27 AM10/21/24
to material...@googlegroups.com
Dear Mr. Kuppasamy,
At high temperatures, you can use UT (using specialized high temperature transducers and couplants 
for internal defects), Eddy Current Test (for surface & subsurface cracks), RT, MPT (with specially 
formulated high-temp inspection mediums for surface and subsurface) and PT ( high temp. penetrants are 
available  for use at 300 deg. C) for surface detections.
The selection  of the NDT method depends on factors like material type, weld configuration, inspection 
accessibility.

Sridhar.
----------------------------------------------------------------------------------------------------------------------------------------


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJg1Sz%3DuqTToO5iiTELw__bb6rQBueKDd_VPNcKTCFQNqqM8bw%40mail.gmail.com.

yamuna ramesh

unread,
Oct 24, 2024, 12:27:16 PM10/24/24
to material...@googlegroups.com
You can select dry method dry powder MPO.